Atomic Layer Deposition (ALD) is a manufacturing method at the atomic and near-atomic scale. Since its invention in the 1970s, ALD has been industrially applied in fields such as displays, semicondu

Related Keywords

Washington ,United States ,Xiao Liu ,Rong Chen ,Key Laboratory Of Intelligent Manufacturing Equipment ,International Journal Of Extreme Manufacturing ,Huazhong University Of Science ,Layer Deposition ,Huazhong University ,International Journal ,Extreme Manufacturing ,State Key Laboratory ,Intelligent Manufacturing Equipment ,Professor Rong Chen ,Space News ,